A Review on challenges and opportunities in wire arc additive manufacturing of aluminium alloys: Specific context of 7xxx series alloys

Main Article Content

Dinesh Wasudeo Rathod
https://orcid.org/0000-0002-3128-8153

Abstract

Wire arc additive manufacturing (WAAM) has emerged as a promising and cost-effective method for producing components made from aluminum alloys, particularly in industries like aviation and aerospace. This process enables the fabrication of high-performance parts while minimizing manufacturing complexities. The demand for aluminum 7xxx series alloys is significant in these sectors due to their outstanding material properties. Efficient production methods, such as WAAM, are essential for utilizing these high-demand materials effectively. Despite the advantages of the WAAM process, challenges remain, particularly when layer-by-layer deposition of Al 7xxx (Al-Zn-Mg) alloys is considered. The high heat density generated during the arcing process can lead to issues such as zinc evaporation, hydrogen formation, and oxidation of the alloys. Additionally, the WAAM technique faces hurdles like delamination, porosity, hot cracking, and complex thermal cycles, all of which can adversely affect the performance of the components produced. This study aims to tackle the challenges associated with the WAAM process by employing Gas Metal Arc Welding techniques, while also exploring opportunities for further research in this area.

Downloads

Download data is not yet available.

Article Details

Section
Articles

References

[1] Z. M. Sun, “Aluminum Alloys in Aerospace Applications,” Journal of Materials Science, vol. 41, no. 3, pp. 707–718, 2006.
[2] B. Zhou, B. Liu, and S. Zhang, “The advancement of 7xxx series aluminum alloys for aircraft structures: A review,” Metals, vol. 11, no. 5, 2021, doi: 10.3390/met11050718.
[3] S. Singh, S. K. Sharma, and D. W. Rathod, “A review on process planning strategies and challenges of WAAM,” Materials Today: Proceedings, vol. 47, pp. 6564–6575, 2020, doi: 10.1016/j.matpr.2021.02.632.
[4] S. Kim and S. K. Moon, “A part consolidation design method for additive manufacturing based on product disassembly complexity,” Applied Sciences (Switzerland), vol. 10, no. 3, 2020, doi: 10.3390/app10031100.
[5] J. Xiong, Y. J. Li, Z. Q. Yin, and H. Chen, “Determination of surface roughness in wire and arc additive manufacturing based on laser vision sensing,” Chinese Journal of Mechanical Engineering (English Edition), vol. 31, no. 4, 2018, doi: 10.1186/s10033-018-0276-8.
[6] M. Gierth, P. Henckell, Y. Ali, J. Scholl, and J. P. Bergmann, “Wire Arc Additive Manufacturing (WAAM) of Aluminum Alloy AlMg5Mn with Energy-Reduced Gas Metal Arc Welding (GMAW),” Materials, vol. 13, no. 12, p. 2671, Jun. 2020, doi: 10.3390/ma13122671.
[7] K. E. K. Vimal, M. Naveen Srinivas, and S. Rajak, “Wire arc additive manufacturing of aluminium alloys: A review,” Materials Today: Proceedings, vol. 41, pp. 1139–1145, 2019, doi: 10.1016/j.matpr.2020.09.153.
[8] M. M. Tawfik, M. M. Nemat-Alla, and M. M. Dewidar, “Enhancing the properties of aluminum alloys fabricated using wire + arc additive manufacturing technique - A review,” Journal of Materials Research and Technology, vol. 13, pp. 754–768, Jul. 2021, doi: 10.1016/j.jmrt.2021.04.076.
[9] S. Li, J. Ning, G. F. Zhang, L. J. Zhang, J. Wu, and L. X. Zhang, “Microstructural and mechanical properties of wire-arc additively manufactured Al–Zn–Mg aluminum alloy: The comparison of as-deposited and heat-treated samples,” Vacuum, vol. 184, 2021, doi: 10.1016/j.vacuum.2020.109860.
[10] B. Wu et al., “Effects of heat accumulation on the arc characteristics and metal transfer behavior in Wire Arc Additive Manufacturing of Ti6Al4V,” Journal of Materials Processing Technology, vol. 250, pp. 304–312, 2017, doi: 10.1016/j.jmatprotec.2017.07.037.
[11] G. K. Mohanta and A. K. Senapati, “The effect of Welding Parameters on Mild Steel by MMAW,” IOP Conference Series: Materials Science and Engineering, vol. 410, no. 1, 2018, doi: 10.1088/1757-899X/410/1/012015.
[12] S. P. Tewari, A. Gupta, and J. Prakash, “Effect of Welding Parameters on the Weldability of Material,” International Journal of Engineering Science and Technology, vol. 2, no. 4, pp. 512–516, 2010.
[13] Z. Afriansyah, M. Ashof, and A. Naimah, “Comparison of SMAW and GTAW Welding Properties,” Mechanics Exploration and Material Innovation, vol. 1, no. 2, pp. 48–53, Apr. 2024, doi: 10.21776/ub.memi.2024.001.02.2.
[14] S. Singh, S. kumar Sharma, and D. W. Rathod, “A review on process planning strategies and challenges of WAAM,” Materials Today: Proceedings, Mar. 2021, doi: 10.1016/j.matpr.2021.02.632.
[15] B. Wu et al., “A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement,” Journal of Manufacturing Processes, vol. 35, pp. 127–139, 2018, doi: 10.1016/j.jmapro.2018.08.001.
[16] D. W. Rathod, J. A. Francis, M. J. Roy, G. Obasi, and N. M. Irvine, “Thermal cycle-dependent metallurgical variations and their effects on the through-thickness mechanical properties in thick section narrow-gap welds,” Materials Science and Engineering A, vol. 707, no. April, pp. 399–411, 2017, doi: 10.1016/j.msea.2017.09.044.
[17] D. W. Rathod, Y. Sun, G. Obasi, and M. J. Roy, “Effect of multiple passes on Lüders/yield plateaus, microstructure and tensile behaviour of narrow-gap thick-section weld plates,” Journal of Materials Science, vol. 54, no. 19, pp. 12833–12850, 2019, doi: 10.1007/s10853-019-03822-z.
[18] L. Wang et al., “Microstructure and mechanical properties of Al-Zn-Mg-Cu alloy fabricated by multi-wire arc-based directed energy deposition,” Journal of Manufacturing Processes, vol. 124, pp. 661–672, 2024, doi: 10.1016/j.jmapro.2024.06.036.
[19] J. Gu, S. Yang, M. Gao, J. Bai, Y. Zhai, and J. Ding, “Micropore evolution in additively manufactured aluminum alloys under heat treatment and inter-layer rolling,” Materials & Design, vol. 186, p. 108288, Jan. 2020, doi: 10.1016/j.matdes.2019.108288.
[20] X. Cai et al., “Microstructure control of ultra-high-strength AlZnMgCu alloys fabricated by wire arc directed energy deposition: the role of variable polarity electric pulse,” Virtual and Physical Prototyping, vol. 19, no. 1, 2024, doi: 10.1080/17452759.2024.2419409.
[21] A. Mauduit, S. Pillot, and H. Gransac, “Study of the suitability of aluminum alloys for additive manufacturing by laser powder-bed fusion,” UPB Scientific Bulletin, Series B: Chemistry and Materials Science, vol. 79, no. 4, pp. 219–238, 2017.
[22] E. O. Olakanmi, R. F. Cochrane, and K. W. Dalgarno, “A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: Processing, microstructure, and properties,” Progress in Materials Science, vol. 74, pp. 401–477, 2015, doi: 10.1016/j.pmatsci.2015.03.002.
[23] K. Bartkowiak, S. Ullrich, T. Frick, and M. Schmidt, “New developments of laser processing aluminium alloys via additive manufacturing technique,” Physics Procedia, vol. 12, no. PART 1, pp. 393–401, 2011, doi: 10.1016/j.phpro.2011.03.050.
[24] N. Kaufmann, M. Imran, T. M. Wischeropp, C. Emmelmann, S. Siddique, and F. Walther, “Influence of process parameters on the quality of aluminium alloy en AW 7075 using Selective Laser Melting (SLM),” Physics Procedia, vol. 83, pp. 918–926, 2016, doi: 10.1016/j.phpro.2016.08.096.
[25] M. L. Montero Sistiaga et al., “Changing the alloy composition of Al7075 for better processability by selective laser melting,” Journal of Materials Processing Technology, vol. 238, pp. 437–445, 2016, doi: 10.1016/j.jmatprotec.2016.08.003.
[26] J. H. Martin, B. D. Yahata, J. M. Hundley, J. A. Mayer, T. A. Schaedler, and T. M. Pollock, “3D printing of high-strength aluminium alloys,” Nature, vol. 549, no. 7672, pp. 365–369, 2017, doi: 10.1038/nature23894.
[27] S. Y. Zhou, Y. Su, H. Wang, J. Enz, T. Ebel, and M. Yan, “Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: Cracking elimination by co-incorporation of Si and TiB2,” Additive Manufacturing, vol. 36, 2020, doi: 10.1016/j.addma.2020.101458.
[28] Q. Tan et al., “A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting,” Materials Science and Engineering: A, vol. 821, 2021, doi: 10.1016/j.msea.2021.141638.
[29] A. Aversa et al., “Laser powder bed fusion of a high strength Al-Si-Zn-Mg-Cu alloy,” Metals, vol. 8, no. 5, 2018, doi: 10.3390/met8050300.
[30] Y. Otani, Y. Kusaki, K. Itagaki, and S. Sasaki, “Microstructure and mechanical properties of A7075 alloy with additional Si objects fabricated by selective laser melting,” Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, vol. 66, no. 3, pp. 109–115, 2019, doi: 10.2497/jjspm.66.109.
[31] Y. Otani and S. Sasaki, “Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability,” Materials Science and Engineering: A, vol. 777, 2020, doi: 10.1016/j.msea.2020.139079.
[32] T. Qi, H. Zhu, H. Zhang, J. Yin, L. Ke, and X. Zeng, “Selective laser melting of Al7050 powder: Melting mode transition and comparison of the characteristics between the keyhole and conduction mode,” Materials and Design, vol. 135, pp. 257–266, 2017, doi: 10.1016/j.matdes.2017.09.014.
[33] B. Mehta et al., “Microstructure, mechanical properties and fracture mechanisms in a 7017 aluminium alloy tailored for powder bed fusion – laser beam,” Materials and Design, vol. 226, 2023, doi: 10.1016/j.matdes.2023.111602.
[34] C. Su, X. Chen, C. Gao, and Y. Wang, “Effect of heat input on microstructure and mechanical properties of Al-Mg alloys fabricated by WAAM,” Applied Surface Science, vol. 486, pp. 431–440, Aug. 2019, doi: 10.1016/j.apsusc.2019.04.255.
[35] G. Liu, J. Xiong, and L. Tang, “Microstructure and mechanical properties of 2219 aluminum alloy fabricated by double-electrode gas metal arc additive manufacturing,” Additive Manufacturing, vol. 35, p. 101375, Oct. 2020, doi: 10.1016/j.addma.2020.101375.
[36] J. Gu et al., “The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy,” Materials Science and Engineering A, vol. 651, pp. 18–26, 2016, doi: 10.1016/j.msea.2015.10.101.
[37] J. Gu, J. Ding, S. W. Williams, H. Gu, P. Ma, and Y. Zhai, “The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys,” Journal of Materials Processing Technology, vol. 230, pp. 26–34, 2016, doi: 10.1016/j.jmatprotec.2015.11.006.
[38] T. Yuan, X. Ren, S. Chen, and X. Jiang, “Grain refinement and property improvements of Al–Zn–Mg–Cu alloy by heterogeneous particle addition during wire and arc additive manufacturing,” Journal of Materials Research and Technology, vol. 16, pp. 824–839, 2022, doi: 10.1016/j.jmrt.2021.12.049.
[39] D. Oropeza et al., “Welding and additive manufacturing with nanoparticle-enhanced aluminum 7075 wire,” Journal of Alloys and Compounds, vol. 834, 2020, doi: 10.1016/j.jallcom.2020.154987.
[40] Y. Guo et al., “Microstructure tuning enables synergistic improvements in strength and ductility of wire-arc additive manufactured commercial Al-Zn-Mg-Cu alloys,” Virtual and Physical Prototyping, vol. 17, no. 3, pp. 649–661, 2022, doi: 10.1080/17452759.2022.2048236.
[41] K. P. Karunakaran, A. Bernard, S. Suryakumar, L. Dembinski, and G. Taillandier, “Rapid manufacturing of metallic objects,” Rapid Prototyping Journal, vol. 18, no. 4, pp. 264–280, 2012, doi: 10.1108/13552541211231644.
[42] A. Singh, A. Ramakrishnan, D. Baker, A. Biswas, and G. P. Dinda, “Laser metal deposition of nickel coated Al 7050 alloy,” Journal of Alloys and Compounds, vol. 719, pp. 151–158, 2017, doi: 10.1016/j.jallcom.2017.05.171.
[43] S. Suryakumar, K. P. Karunakaran, A. Bernard, U. Chandrasekhar, N. Raghavender, and D. Sharma, “Weld bead modeling and process optimization in Hybrid Layered Manufacturing,” CAD Computer Aided Design, vol. 43, no. 4, pp. 331–344, 2011, doi: 10.1016/j.cad.2011.01.006.
[44] J. K. Yoder, R. J. Griffiths, and H. Z. Yu, “Deformation-based additive manufacturing of 7075 aluminum with wrought-like mechanical properties,” Materials and Design, vol. 198, 2021, doi: 10.1016/j.matdes.2020.109288.
[45] J. Gu, M. Gao, S. Yang, J. Bai, Y. Zhai, and J. Ding, “Microstructure, defects, and mechanical properties of wire + arc additively manufactured Al[sbnd]Cu4.3-Mg1.5 alloy,” Materials and Design, vol. 186, 2020, doi: 10.1016/j.matdes.2019.108357.
[46] R. Sun et al., “Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening,” Journal of Alloys and Compounds, vol. 747, pp. 255–265, May 2018, doi: 10.1016/j.jallcom.2018.02.353.
[47] J. Gu, J. Bai, J. Ding, S. Williams, L. Wang, and K. Liu, “Design and cracking susceptibility of additively manufactured Al-Cu-Mg alloys with tandem wires and pulsed arc,” Journal of Materials Processing Technology, vol. 262, pp. 210–220, 2018, doi: 10.1016/j.jmatprotec.2018.06.030.
[48] S. C. Altıparmak, V. A. Yardley, Z. Shi, and J. Lin, “Challenges in additive manufacturing of high-strength aluminium alloys and current developments in hybrid additive manufacturing,” International Journal of Lightweight Materials and Manufacture, vol. 4, no. 2, pp. 246–261, 2021, doi: 10.1016/j.ijlmm.2020.12.004.
[49] W. Ou, T. Mukherjee, G. L. Knapp, Y. Wei, and T. DebRoy, “Fusion zone geometries, cooling rates and solidification parameters during wire arc additive manufacturing,” International Journal of Heat and Mass Transfer, vol. 127, pp. 1084–1094, 2018, doi: 10.1016/j.ijheatmasstransfer.2018.08.111.
[50] J. W. Elmer and G. Gibbs, “The effect of atmosphere on the composition of wire arc additive manufactured metal components,” Science and Technology of Welding and Joining, vol. 24, no. 5, pp. 367–374, 2019, doi: 10.1080/13621718.2019.1605473.
[51] H. Zhang, H. Zhu, T. Qi, Z. Hu, and X. Zeng, “Selective laser melting of high strength Al-Cu-Mg alloys: Processing, microstructure and mechanical properties,” Materials Science and Engineering: A, vol. 656, pp. 47–54, 2016, doi: 10.1016/j.msea.2015.12.101.
[52] T. Soysal and S. Kou, “A simple test for assessing solidification cracking susceptibility and checking validity of susceptibility prediction,” Acta Materialia, vol. 143, pp. 181–197, 2018, doi: 10.1016/j.actamat.2017.09.065.
[53] A. Aversa et al., “New aluminum alloys specifically designed for laser powder bed fusion: A review,” Materials, vol. 12, no. 7, 2019, doi: 10.3390/ma12071007.
[54] B. Cong, J. Ding, and S. Williams, “Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy,” International Journal of Advanced Manufacturing Technology, vol. 76, no. 9–12, pp. 1593–1606, 2015, doi: 10.1007/s00170-014-6346-x.
[55] P. Edwards, A. O’Conner, and M. Ramulu, “Electron beam additive manufacturing of titanium components: Properties and performance,” Journal of Manufacturing Science and Engineering, vol. 135, no. 6, 2013, doi: 10.1115/1.4025773.
[56] P. N. Anyalebechi, “Hydrogen-induced gas porosity formation in Al-4.5 wt% Cu-1.4 wt% Mg alloy,” Journal of Materials Science, vol. 48, no. 15, pp. 5342–5353, 2013, doi: 10.1007/s10853-013-7329-2.
[57] X. Guo et al., “Enhancing strength, ductility, and fatigue performance of Al-Zn-Mg-Cu-Sc-Zr alloy using a hybrid approach: Wire-arc directed energy deposition and interlayer friction stir processing,” Journal of Materials Processing Technology, vol. 322, 2023, doi: 10.1016/j.jmatprotec.2023.118173.
[58] A. P. Boeira, I. L. Ferreira, and A. Garcia, “Alloy composition and metal/mold heat transfer efficiency affecting inverse segregation and porosity of as-cast Al-Cu alloys,” Materials and Design, vol. 30, no. 6, pp. 2090–2098, 2009, doi: 10.1016/j.matdes.2008.08.032.
[59] J. L. Gu et al., “The Influence of Wire Properties on the Quality and Performance of Wire+Arc Additive Manufactured Aluminium Parts,” Advanced Materials Research, vol. 1081, pp. 210–214, 2014, doi: 10.4028/www.scientific.net/amr.1081.210.
[60] M. M. Tawfik, M. M. Nemat-Alla, and M. M. Dewidar, “Enhancing the properties of aluminum alloys fabricated using wire + arc additive manufacturing technique - A review,” Journal of Materials Research and Technology, vol. 13, pp. 754–768, 2021, doi: 10.1016/j.jmrt.2021.04.076.
[61] A. Busachi, J. Erkoyuncu, P. Colegrove, F. Martina, and J. Ding, “Designing a WAAM based manufacturing system for defence applications,” Procedia CIRP, vol. 37, pp. 48–53, 2015, doi: 10.1016/j.procir.2015.08.085.
[62] E. R. Denlinger, J. Irwin, and P. Michaleris, “Thermomechanical modeling of additive manufacturing large parts,” Journal of Manufacturing Science and Engineering, Transactions of the ASME, vol. 136, no. 6, 2014, doi: 10.1115/1.4028669.
[63] J. Mehnen, J. Ding, H. Lockett, and P. Kazanas, “Design study for wire and arc additive manufacture,” International Journal of Product Development, vol. 19, no. 1–3, pp. 2–20, 2014, doi: 10.1504/IJPD.2014.060028.
[64] X. Tan et al., “Graded microstructure and mechanical properties of additive manufactured Ti-6Al-4V via electron beam melting,” Acta Materialia, vol. 97, pp. 1–16, 2015, doi: 10.1016/j.actamat.2015.06.036.
[65] V. T. Le, D. S. Mai, T. K. Doan, and H. Paris, “Wire and arc additive manufacturing of 308L stainless steel components: Optimization of processing parameters and material properties,” Engineering Science and Technology, an International Journal, vol. 24, no. 4, pp. 1015–1026, 2021, doi: 10.1016/j.jestch.2021.01.009.
[66] H. Y. Jung, N. J. Peter, E. Gärtner, G. Dehm, V. Uhlenwinkel, and E. A. Jägle, “Bulk nanostructured AlCoCrFeMnNi chemically complex alloy synthesized by laser-powder bed fusion,” Additive Manufacturing, vol. 35, 2020, doi: 10.1016/j.addma.2020.101337.
[67] Z. Hu, X. Nie, Y. Qi, H. Zhang, and H. Zhu, “Cracking criterion for high strength Al–Cu alloys fabricated by selective laser melting,” Additive Manufacturing, vol. 37, 2021, doi: 10.1016/j.addma.2020.101709.
[68] Q. Tan et al., “A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles,” Additive Manufacturing, vol. 32, 2020, doi: 10.1016/j.addma.2019.101034.
[69] D. Gu and Y. Shen, “Balling phenomena during direct laser sintering of multi-component Cu-based metal powder,” Journal of Alloys and Compounds, vol. 432, no. 1–2, pp. 163–166, 2007, doi: 10.1016/j.jallcom.2006.06.011.
[70] D. Wu et al., “Al–Cu alloy fabricated by novel laser-tungsten inert gas hybrid additive manufacturing,” Additive Manufacturing, vol. 32, 2020, doi: 10.1016/j.addma.2019.100954.
[71] I. Yadroitsev, P. Krakhmalev, I. Yadroitsava, S. Johansson, and I. Smurov, “Energy input effect on morphology and microstructure of selective laser melting single track from metallic powder,” Journal of Materials Processing Technology, vol. 213, no. 4, pp. 606–613, 2013, doi: 10.1016/j.jmatprotec.2012.11.014.
[72] E. Louvis, P. Fox, and C. J. Sutcliffe, “Selective laser melting of aluminium components,” Journal of Materials Processing Technology, vol. 211, no. 2, pp. 275–284, 2011, doi: 10.1016/j.jmatprotec.2010.09.019.
[73] A. Heinz, A. Haszler, C. Keidel, S. Moldenhauer, R. Benedictus, and W. S. Miller, “Recent development in aluminium alloys for aerospace applications,” Materials Science and Engineering: A, vol. 280, no. 1, pp. 102–107, 2000, doi: 10.1016/S0921-5093(99)00674-7.
[74] K. S. Derekar, “A review of wire arc additive manufacturing and advances in wire arc additive manufacturing of aluminium,” Materials Science and Technology (United Kingdom), vol. 34, no. 8, pp. 895–916, 2018, doi: 10.1080/02670836.2018.1455012.
[75] N. T. Aboulkhair, M. Simonelli, L. Parry, I. Ashcroft, C. Tuck, and R. Hague, “3D printing of Aluminium alloys: Additive Manufacturing of Aluminium alloys using selective laser melting,” Progress in Materials Science, vol. 106, p. 100578, Dec. 2019, doi: 10.1016/j.pmatsci.2019.100578.